MC-Injekt 2700 L: How Polyurethane Crack Injection Seals and Strengthens Leaking Concrete

Water seeping through a crack in a basement wall, lift pit or underground water tank is more than a cosmetic problem. Over time, moisture corrodes reinforcement, weakens concrete and damages finishes and stored goods. Surface coatings may hide the dampness for a while, but when water is travelling through the crack itself, the lasting fix is to fill that path from within. Crack injection with MC-Bauchemie MC-Injekt 2700 L is designed to do exactly that.

What Is MC-Injekt 2700 L?

MC-Injekt 2700 L is a two-component, low-viscosity injection resin based on polyurethane, made by German construction chemicals manufacturer MC-Bauchemie. Once cured, it becomes a rigid duromer with high compressive and tensile strength. That gives it a dual role: it seals cracks and voids against water, and it restores a force-locking bond across cracked structural elements.

The “L” variant offers a longer working time than standard MC-Injekt 2700, which helps when injecting long cracks, deep voids or larger volumes in one continuous operation.

How Does It Work?

The resin is pumped under pressure into the crack through injection packers. Its low viscosity lets it travel into fine cracks and capillaries that thicker materials cannot reach. Two properties make it especially effective on wet sites:

  • Water-displacing behaviour: The resin pushes water out of the crack as it advances, so it can be used on damp and water-bearing structures.
  • Controlled foaming: On contact with water, it forms only a limited amount of hard, closed-cell foam rather than a soft expanding foam, preserving strength while filling the void.

Reaction time can be adjusted on site. Adding the MC-KAT 27 accelerator speeds up the reaction, while MC-Additiv ST increases thixotropy so the resin stays in place in wider cracks and voids.

Where Is MC-Injekt 2700 L Used?

  • Cracked basement walls, raft slabs and retaining walls
  • Underground water tanks, sumps and lift pits
  • Tunnels, culverts, channels and other hydraulic structures
  • Honeycombed concrete and voids around poorly compacted construction joints
  • Cracked masonry and natural stone structures
  • Sealing excavation pit enclosures and foundation soil

Key Benefits

  • Durable, long-term water impermeability
  • High compressive and tensile strength for structural restoration
  • Good injectability into fine cracks
  • Adjustable reactivity to suit changing site conditions
  • Suitable for dry, damp and water-bearing cracks

The Injection Process: Step by Step

  1. Inspect and plan. Map the cracks, note whether they are dry, damp or actively leaking, and confirm that the movement that caused them has stopped. A rigid resin works best on cracks that are no longer moving.
  2. Drill and fix packers. Drill holes at an angle so they intersect the crack, usually staggered on alternate sides, and install suitable injection packers.
  3. Seal the surface if required. Sealing open crack faces prevents resin loss and drives the material into the full depth of the crack.
  4. Using a two-component injection pump with a static mixer, inject from the lowest packer upwards, moving to the next packer once resin appears there.
  5. After curing, remove or cut back the packers and repair the drill holes with a suitable mortar.
  6. Clean the equipment. Flush the pump with MC-Verdünnung PU. Never use water or water-based cleaners, which react with the resin.

Rigid vs. Flexible Injection: Choosing Correctly

MC-Injekt 2700 L is the right choice when a crack is static and you need both sealing and structural bonding. If a crack or joint continues to move with temperature or load, a flexible injection resin is more appropriate, because the crack may reopen next to a rigid repair. Where water is gushing under high pressure, a fast-reacting water-stop resin may be needed first to control the flow. A specialist assessment before work begins saves time and avoids repeat repairs.

Part of a Complete Waterproofing Strategy

Crack injection treats existing leak paths, but long-term protection depends on the overall system. For new basements, consider a crystalline waterproofing system that seals capillaries within the concrete, or an HDPE waterproofing membrane for substructures on the positive side. Using the right concrete admixtures from the start reduces shrinkage cracking and permeability. For a broader overview, read our guide on the best waterproofing solution for basement construction in India. Above ground, a flexible coating such as MAPEI Mapelastic Smart protects terraces and wet areas.

Conclusion

MC-Injekt 2700 L offers a proven way to stop water ingress through cracks while restoring structural integrity. Its low viscosity, water-displacing action and extended working time make it a dependable choice for basements, tanks, tunnels and foundations. Explore MC-Injekt 2700 L at Crete Pro Trading or speak to our team about the right injection approach for your structure.

Frequently Asked Questions

1. What is MC-Injekt 2700 L?

MC-Injekt 2700 L is a two-component, low-viscosity polyurethane injection resin from MC-Bauchemie. It cures into a rigid duromer that permanently seals cracks and voids in concrete, masonry and foundation soil while restoring structural strength.

2. What is the difference between MC-Injekt 2700 and MC-Injekt 2700 L?

Both are rigid polyurethane resins for sealing and strengthening cracked structures. The L version offers a longer working time, which is useful for long cracks, deep voids and larger injection volumes.

3. Can MC-Injekt 2700 L be used on actively leaking cracks?

Yes. The resin is water-displacing and forms a limited amount of hard foam on contact with water, so it can be injected into damp and water-bearing cracks. Where water flows under high pressure, a fast-reacting water-stop resin may be needed first.

4. Is MC-Injekt 2700 L suitable for moving cracks or expansion joints?

No. Because it cures rigid, it is intended for static cracks. Cracks and joints that continue to move should be treated with a flexible injection resin or a suitable joint sealing system.

5. What equipment is required to apply MC-Injekt 2700 L?

It is applied with a two-component injection pump fitted with a static mixer, along with suitable injection packers. Equipment must be cleaned with MC-Verdünnung PU and never with water or water-based cleaners.